Tag Archives: reflow soldering

IPC Video Team Shoots Two New Videos at Delta Group Electronics

IPC recently shot two new training videos at Delta Group Electronics in Albuquerque, New Mexico, “Safety in Electronics Assembly” and “Convection Reflow Soldering.” Both of these programs will soon be available in the new IPC EDGE 2.0 Online Video Training Library. Tod Cummins, Delta Group’s Director of Corporate Quality was responsible for arranging and coordinating […]

Defect of the Month from NPL and IPC: Solder Wicking and Reflow

Fine pitch components, convection reflow with nitrogen, and vapor phase reflow can all add up to solder wicking where the solder is drawn to either the component terminations or the pads. Industry expert Bob Willis explains the causes in this video from the National Physical Laboratory Defect Database. The defect database allows engineers to search […]