IPC standards committee reports: materials, boards, embedded, flex

This is part of a series of updates from IPC standards committee meetings at IPC Midwest. Base Materials The 3-11 Laminate/Prepreg Materials Subcommittee worked on amending IPC-4101C, Specification for Base Materials for Rigid and Multilayer Printed Boards. Proposed items for inclusion were: a) adding DMA thermal analysis testing for measurement of Tg; b) inserting the […]

IPC Standards Committees: Progress Reports for Board Design, Fabrication and Related Areas

Keep up with IPC standards committee activities with these status reports published in our recent Intouch Newsletter. For more information on a particular committee, visit our committee home pages , the IPC status of standardization or e-mail answers@ipc.org. Printed Board Design The 1-10C Test Coupon and Artwork Generation Task Group approved Appendix A to IPC-2221B, […]